Stable Electrode/Electrolyte Interface for High-Voltage NCM 523 Cathode Constructed by Synergistic Positive and Passive Approaches

Тип публикацииJournal Article
Дата публикации2021-11-19
scimago Q1
wos Q1
БС1
SJR1.921
CiteScore14.5
Impact factor8.2
ISSN19448244, 19448252
General Materials Science
Краткое описание
Increasing the working voltage of lithium-ion batteries (LIBs) is an efficient way to increase energy density. However, high voltage triggers excessive electrolyte decomposition at the electrode-electrolyte interfaces, where the electrochemical performance such as cyclic stability and rate capability is seriously deteriorated. A new synergistic positive and passive approach is proposed in this work to construct a stable electrode-electrolyte interface at high voltage. As a positive approach, inorganic lithium sulfide salt (Li2S) is used as an electrolyte additive to build a stable cathode electrolyte interface (CEI) at the LiNi0.5Co0.2Mn0.3O2 (NCM523) cathode surface. In a passive way, acetonitrile (AN) is applied as a solvent additive to suppress oxidative decomposition of a carbonate electrolyte via preferential solvation with a lithium ion. Because of the synergistic interaction between the positive and passive approaches, the cyclic stabilities of NCM523/Li cells improved with a tiny amount of Li2S (0.01 mg mL-1) and AN (0.5 vol %). The capacity retention increased to 80.74% after 200 cycles compared to the cells with the blank electrolyte (67.98%) and AN-containing electrolyte (75.8%). What is more, the capacity retention of the NCM523/graphite full cell is increased from 65 to 81% with the addition of the same amount of Li2S and AN after 180 cycles. The mechanism is revealed on the basis of the theoretical calculations and various characterizations. The products derived from the preferential adsorption and oxidation of Li2S on the surface of NCM523 effectively increase the content of inorganic ingredients. However, the presence of AN prevents oxidation of the solvent. This study provides new principle guiding studies on a high-voltage lithium-ion battery with excellent electrochemical performance.
Найдено 
Для доступа к списку цитирований публикации необходимо авторизоваться.
Для доступа к списку профилей, цитирующих публикацию, необходимо авторизоваться.

Топ-30

Журналы

1
2
3
4
Journal of Power Sources
4 публикации, 8.51%
ACS Applied Energy Materials
3 публикации, 6.38%
Energy Storage Materials
3 публикации, 6.38%
ACS applied materials & interfaces
3 публикации, 6.38%
Electrochimica Acta
2 публикации, 4.26%
Applied Surface Science
2 публикации, 4.26%
Journal of Colloid and Interface Science
2 публикации, 4.26%
Mendeleev Communications
1 публикация, 2.13%
ACS Nano
1 публикация, 2.13%
Energies
1 публикация, 2.13%
Batteries
1 публикация, 2.13%
Chemical Engineering Journal
1 публикация, 2.13%
Energy Technology
1 публикация, 2.13%
Journal of Physical Chemistry Letters
1 публикация, 2.13%
Journal of Materials Science
1 публикация, 2.13%
Nano Research
1 публикация, 2.13%
ACS Energy Letters
1 публикация, 2.13%
Journal of Energy Storage
1 публикация, 2.13%
ACS Omega
1 публикация, 2.13%
Small
1 публикация, 2.13%
Journal of Physical Chemistry C
1 публикация, 2.13%
Materials
1 публикация, 2.13%
Angewandte Chemie - International Edition
1 публикация, 2.13%
Angewandte Chemie
1 публикация, 2.13%
Advanced Energy and Sustainability Research
1 публикация, 2.13%
Advanced Materials
1 публикация, 2.13%
Energy Materials
1 публикация, 2.13%
Composites Part B: Engineering
1 публикация, 2.13%
Nature Reviews Chemistry
1 публикация, 2.13%
Ceramics International
1 публикация, 2.13%
1
2
3
4

Издатели

2
4
6
8
10
12
14
16
18
20
Elsevier
19 публикаций, 40.43%
American Chemical Society (ACS)
12 публикаций, 25.53%
Wiley
6 публикаций, 12.77%
MDPI
3 публикации, 6.38%
Springer Nature
3 публикации, 6.38%
OOO Zhurnal "Mendeleevskie Soobshcheniya"
1 публикация, 2.13%
OAE Publishing Inc.
1 публикация, 2.13%
Wuhan University of Technology
1 публикация, 2.13%
Royal Society of Chemistry (RSC)
1 публикация, 2.13%
2
4
6
8
10
12
14
16
18
20
  • Мы не учитываем публикации, у которых нет DOI.
  • Статистика публикаций обновляется еженедельно.

Вы ученый?

Создайте профиль, чтобы получать персональные рекомендации коллег, конференций и новых статей.
Метрики
47
Поделиться
Цитировать
ГОСТ |
Цитировать
Shi X. et al. Stable Electrode/Electrolyte Interface for High-Voltage NCM 523 Cathode Constructed by Synergistic Positive and Passive Approaches // ACS applied materials & interfaces. 2021. Vol. 13. No. 48. pp. 57107-57117.
ГОСТ со всеми авторами (до 50) Скопировать
Shi X., Zheng T., Xiong J., Zhu B., Cheng Y., Liu Z. Stable Electrode/Electrolyte Interface for High-Voltage NCM 523 Cathode Constructed by Synergistic Positive and Passive Approaches // ACS applied materials & interfaces. 2021. Vol. 13. No. 48. pp. 57107-57117.
RIS |
Цитировать
TY - JOUR
DO - 10.1021/acsami.1c15690
UR - https://doi.org/10.1021/acsami.1c15690
TI - Stable Electrode/Electrolyte Interface for High-Voltage NCM 523 Cathode Constructed by Synergistic Positive and Passive Approaches
T2 - ACS applied materials & interfaces
AU - Shi, Xiaotang
AU - Zheng, Tianle
AU - Xiong, Jianwei
AU - Zhu, Bingying
AU - Cheng, Yajun
AU - Liu, Zhaoping
PY - 2021
DA - 2021/11/19
PB - American Chemical Society (ACS)
SP - 57107-57117
IS - 48
VL - 13
PMID - 34797642
SN - 1944-8244
SN - 1944-8252
ER -
BibTex |
Цитировать
BibTex (до 50 авторов) Скопировать
@article{2021_Shi,
author = {Xiaotang Shi and Tianle Zheng and Jianwei Xiong and Bingying Zhu and Yajun Cheng and Zhaoping Liu},
title = {Stable Electrode/Electrolyte Interface for High-Voltage NCM 523 Cathode Constructed by Synergistic Positive and Passive Approaches},
journal = {ACS applied materials & interfaces},
year = {2021},
volume = {13},
publisher = {American Chemical Society (ACS)},
month = {nov},
url = {https://doi.org/10.1021/acsami.1c15690},
number = {48},
pages = {57107--57117},
doi = {10.1021/acsami.1c15690}
}
MLA
Цитировать
Shi, Xiaotang, et al. “Stable Electrode/Electrolyte Interface for High-Voltage NCM 523 Cathode Constructed by Synergistic Positive and Passive Approaches.” ACS applied materials & interfaces, vol. 13, no. 48, Nov. 2021, pp. 57107-57117. https://doi.org/10.1021/acsami.1c15690.